The marine immersion corrosion of irons and steel under calcareous deposition (principally calcium carbonate) is known to be relatively low for shorter exposures (e.g., a few years). Herein the effect of calcareous deposition on corrosion is considered for exposures up to 1,300 y. The data are derived from archaeological steel and iron shipwrecks, cast iron cannons and cannonballs, and wrought iron anchors in locations where there was direct evidence, in and on the corrosion products, of calcareous deposition. Such deposition promotes formation of calcium and ferrous carbonate layers of low permeability on and within rusts. These tend to inhibit both early and long-term corrosion rates. The data show that up to about 200 y exposure corrosion losses as a function of time can be approximated closely by a linear function of time. Longer exposures follow a moderate power-law function, consistent with diffusion considerations. Comments are made about the likely interplay between calcareous deposition and microbiological corrosion.
Skip Nav Destination
Article navigation
1 May 2021
Research Article|
February 16 2021
Long-Term Immersion Corrosion of Irons and Steel in Seawaters with Calcareous Deposition
R.E. Melchers
R.E. Melchers
‡
Centre for Infrastructure Performance and Reliability, The University of Newcastle, Callaghan, Australia.
‡Corresponding author. E-mail: [email protected].
Search for other works by this author on:
CORROSION (2021) 77 (5): 526–539.
Citation
R.E. Melchers; Long-Term Immersion Corrosion of Irons and Steel in Seawaters with Calcareous Deposition. CORROSION 1 May 2021; 77 (5): 526–539. doi: https://doi.org/10.5006/3685
Download citation file:
Sign in
Don't already have an account? Register
Client Account
You could not be signed in. Please check your email address / username and password and try again.
Could not validate captcha. Please try again.
Sign in via your Institution
Sign in via your InstitutionCiting articles via
Key Challenges for Internal Corrosion Modelling of Wet Gas Pipelines
N. Laycock, V. Metri, S. Rai, A. Sabhapondit, J. Hartog, S. Ghosh, A.M. Abdullah
Development of Accelerated Galvanic Corrosion Testing for Evaluating Heat Exchanger Corrosion Penetration Lifespan
Eun-Ha Park, Jeong-Min Lim, Geon-Il Kim, Yong-Won Kim, Jung-Gu Kim
Improving the Long—Term Protection of Buried Steel Tanks: Considering the Impact of Temperature and Extended Sacrificial Anodes
Mohammad Javad Shirshahi, Seyed Farshid Chini, Peyman Taheri, Abraham Mansouri
Corrosion prediction model for long-distance pipelines based on NLFE-NGO-ELM
Xingyu Du, Yujie Dai, Bailing Zheng, Xinqi Zhu
Identification of Synergistic Interactions in Green Corrosion Inhibitor Mixtures by Molecular Modeling
Carlos M. Menendez, Oleg A. Mazyar, Sunder Ramachandran, Tracey Jackson