FIGURE 6.
(a) BSE and (b, c) WDS elemental maps of DED 304L exhibiting retained intracellular δ ferrite with elevated Cr and Ni content; SE image of the same material after a double-loop electrochemical polarization resistance test showing trenching of austenite surrounding the δ ferrite (bright). Reprinted from Melia, et al.18

(a) BSE and (b, c) WDS elemental maps of DED 304L exhibiting retained intracellular δ ferrite with elevated Cr and Ni content; SE image of the same material after a double-loop electrochemical polarization resistance test showing trenching of austenite surrounding the δ ferrite (bright). Reprinted from Melia, et al.18 